Item | Standard or Method | Test Result | ||
Impact Resistance Test | ISO6272 | GB/T1732-1993 | 50cm | |
Cupping Test | ISO1520 | GB/T9753-1988 | 7mm | |
Adhesion Test (Cross cut ) | ISO2409 | GB/T9286-1998 | Gt.0 | |
Bend Test | ISO1519 | GB/T6742-1986 | 2mm | |
Hardness Test | ISO15184 | GB/T6739-1996 | 1H-2H | |
Salt Spary | ISO7253 | GB/T1771-1991 | >800h | |
Damp Hot Test | ISO6270 | GB/T1740-1979 | >1000h | |
Heat Resistance |
140ºC/24h (white) |
gloss retention ΔE≤0.3-0.4 |
||
Weathering Durability |
Florida |
ISO2810 |
Facing south 45° 12month |
Gloss retention :≥50% |
Accelerated aging |
60ºC/8 h UV+50ºC/4 h condensation,cycling500h |
Gloss retention:≥50% color stability:ΔE≤3.5 |
||